Kandungan Kimia, %
| Ni | Mn | Fe | Si | Cu | Anu sanésna | Diréktif ROHS | |||
| Cd | Pb | Hg | Cr | ||||||
| 44 | 1,50% | 0.5 | - | Bal | - | ND | ND | ND | ND |
Sipat Mékanis
| Suhu Layanan Kontinyu Maks. | 400ºC |
| Résistivitas dina 20ºC | 0,49±5%ohm mm2/m |
| Kapadetan | 8,9 g/cm3 |
| Konduktivitas Termal | -6 (Maks) |
| Titik Lebur | 1280ºC |
| Kakuatan Tarik, N/mm2 Dipanaskeun, Lemes | 340~535 Mpa |
| Kakuatan Tarik, N/mm3 Digulung Tiis | 680~1070 Mpa |
| Elongasi (anil) | 25% (Min) |
| Elongasi (digulung tiis) | ≥Min)2%(Min) |
| EMF vs Cu, μV/ºC (0~100ºC) | -43 |
| Struktur Mikrografik | austenit |
| Sipat Magnét | Henteu |
150 0000 2421