| Ni | Mn | Fe | Si | Cu | Lain | Diréktif ROHS | |||
| Cd | Pb | Hg | Cr | ||||||
| 23 | 0.5 | - | - | Bal | - | ND | ND | ND | ND |
Sipat mékanis
| Max Kontinyu Service Temp | 300ºC |
| Résistivitas dina 20ºC | 0,30 ohm mm2 / m |
| Kapadetan | 8,9 g/cm3 |
| Konduktivitas termal | 16 (Max) |
| Titik lebur | 1150ºC |
| Kakuatan Tensile, N/mm2 Annealed, Lemes | 350~420 Mpa |
| Kakuatan Tensile, N / mm2 Tiis Digulung | 380~840 Mpa |
| Elongation (anil) | 25% (Max) |
| Elongation (digulung tiis) | 2% (Max) |
| EMF vs Cu, μV/ºC (0~100ºC) | -30 |
| Struktur Mikrografi | austenit |
| Harta magnét | Henteu |
Ngaran Dagang CuNi23Mn:
Alloy 180, CuNi 180, 180 Alloy, MWS-180, Cuprothal 180, Midohm, HAI-180, Cu-Ni 23, Alloy 380, Nikel alloy 180
150 0000 2421