ferroalloys 0Cr21Al6Nb kawat lalawanan fecral pikeun kompor listrik
Kelas | 0Cr21Al6NbCo |
Ukuran | 0,1-1,2 mm |
Beungeut | annealed caang |
Beurat | 1-3 kg/gulungan |
Résistansi | 1,45±0,07μΩ.m |
Suhu pangluhurna | 1350 ℃ |
Kapadetan | 7,1 g/cm³ |
Kakuatan regangan | 750N/mm² |
Elongation | ≥12% |
Kelas | Suhu pangluhurna | Résistansi | Titik lebur | Kakuatan regangan | Elongation |
0Cr21Al4 | 1100 ℃ | 1,23±0,06μΩ.m | 1500 ℃ | 750 | ≥12 |
0Cr25Al5 | 1250 ℃ | 1,42±0,07μΩ.m | 1500 ℃ | 750 | ≥12 |
0Cr23Al5 | 1300 ℃ | 1,35±0,06μΩ.m | 1500 ℃ | 750 | ≥12 |
0Cr21Al6NbCo | 1350 ℃ | 1,45±0,07μΩ.m | 1510 ℃ | 750 | ≥12 |
0Cr27Al7Mo2 | 1400 ℃ | 1,53±0,07μΩ.m | 1520 ℃ | 750 | ≥10 |
KSC | 1350 ℃ | 1,44±0,05μΩ.m | 1510 ℃ | 750 | ≥16 |
Cr20Ni80 | 1200 ℃ | 1,09±0,05μΩ.m | 1400 ℃ | 750 | ≥20 |
Cr15Ni60 | 1150 ℃ | 1,12±0,05μΩ.m | 1390 ℃ | 750 | ≥20 |
Cr20Ni35 | 1100 ℃ | 1,04±0,05μΩ.m | 1390 ℃ | 750 | ≥20 |
Cr20Ni30 | 1100 ℃ | 1,04±0,05μΩ.m | 1390 ℃ | 750 | ≥20 |
Kelas | Komposisi kimia% | ||||||||
C | P | S | Mn | Si | Cr | Ni | Al | Fe | |
≤ | |||||||||
0Cr21Al4 | 0.12 | 0,025 | 0,025 | 0.7 | ≤1.0 | 17-21 | ≤0.6 | 3-4 | kasaimbangan |
0Cr25Al5 | 0.06 | 0,025 | 0.02 | 0.5 | ≤0.6 | 23-26 | ≤0.6 | 4.5-6.5 | kasaimbangan |
0Cr23Al5 | 0.06 | 0,025 | 0.02 | 0.5 | ≤0.6 | 20.5-23.5 | ≤0.6 | 4.2-5.3 | kasaimbangan |
0Cr21Al6Nb | 0.05 | 0,025 | 0.02 | 0.5 | ≤0.6 | 21-23 | ≤0.6 | 5-7 | kasaimbangan |
0Cr27Al7Mo2 | 0.05 | 0,025 | 0.02 | 0.2 | ≤0.4 | 26.5-27.8 | ≤0.6 | 6-7 | kasaimbangan |
Cr20Ni80 | 0.08 | 0.02 | 0,015 | 0.6 | 0.75-1.6 | 20-23 | kasaimbangan | <0,5 | ≤1.0 |
Cr15Ni60 | 0.08 | 0.02 | 0,015 | 0.6 | 0.75-1.6 | 15-18 | 55-61 | <0,5 | kasaimbangan |
Cr20Ni35 | 0.08 | 0.02 | 0,015 | 1.0 | 1-3 | 18-21 | 34-37 | - | kasaimbangan |
Cr20Ni30 | 0.08 | 0.02 | 0,015 | 1.0 | 1-3 | 18-21 | 30-34 | - | kasaimbangan |