| Kelas | 0Cr21Al6Nb |
| Ukuran | ketebalan: 0.05-3mm lébar: 4-250mm |
| Beungeut | motongan anu caang |
| Beurat | 5-200kg/gulungan, numutkeun kuantitas konsumén |
| Résistansi | 1,45±0,05μΩ.m |
| Teuas (HV) | 200-240HV |
| Pemanjangan | ≥12% |
Parameter Produksi
| Kelas | Suhu pangluhurna | Résistansi | Karasa | Kakuatan regangan | Pemanjangan |
| 0Cr13Al4 | 1050ºC | 1,25±0,05μΩ.m | 180-210HV | ≥550N/mm2 | ≥16 |
| 0Cr15Al5 | 1100ºC | 1.3±0.05μΩ.m | 180-210HV | ≥550N/mm2 | ≥16 |
| 0Cr21Al6Nb | 1300ºC | 1,42±0,05μΩ.m | 200-240HV | 750N/mm2 | ≥12 |
| Cr20Ni80 | 1200ºC | 1,09±0,05μΩ.m | 180-220HV | 750N/mm2 | ≥20 |
| Cr15Ni60 | 1150ºC | 1.12±0.05μΩ.m | 175-210HV | 750N/mm2 | ≥20 |
| Cr20Ni35 | 1100ºC | 1,04±0,05μΩ.m | 180-220HV | 750N/mm2 | ≥20 |
| Cr25Ni20 | 1100ºC | 0,86±0,05μΩ.m | 180-220HV | 750N/mm2 | ≥20 |
| Kelas | Komposisi kimia% | ||||||||
| C | P | S | Mn | Si | Cr | Ni | Al | Fe | |
| ≤ | |||||||||
| 0Cr15Al5 | 0.04 | 0.02 | 0.01 | 0.3 | ≤0.5 | 13-14 | <1 | 4.8-5.0 | kasaimbangan |
| 0Cr21Al6Nb | 0.05 | 0.025 | 0.02 | 0.5 | ≤0.6 | 21-23 | ≤0.6 | 5-7 | kasaimbangan |
| 0Cr13Al4 | 0.04 | 0.02 | 0.01 | 0.3 | ≤0.5 | 13-14 | <1 | 4.8-5.0 | kasaimbangan |
| Cr20Ni80 | 0.08 | 0.02 | 0.015 | 0.6 | 0.75-1.6 | 20-23 | kasaimbangan | <0.5 | ≤1.0 |
| Cr15Ni60 | 0.08 | 0.02 | 0.015 | 0.6 | 0.75-1.6 | 15-18 | 55-61 | <0.5 | kasaimbangan |
| Cr20Ni35 | 0.08 | 0.02 | 0.015 | 1.0 | 1-3 | 18-21 | 34-37 | - | kasaimbangan |
| Cr25Ni20 | 0.08 | 0.045 | 0.03 | 2.0 | 0.4-0.6 | 24-26 | 19-22 | - | kasaimbangan |