Séng Murni/Monel 400/Tafa 70t/Monel K500/Ernicu-7/Ni95al5/Tafa 75b/Hastalloy C-276Kawat Semprot Termal Stainless Steel
Panjelasan Produk
1. FM60 Oxford Alloy 60ERNiCu-7rod las TIG
ERNiCu-7 gaduh kakuatan anu saé sareng tahan korosi dina seueur média, kalebet cai laut, uyah, sareng asam réduksi. Sarta eta bisa dipaké pikeun overlay leuwih baja karbon, disadiakeun lapisan panyangga of ERNi-1 dipaké pikeun lapisan kahiji. alloy Ieu teu umur hardnable sarta lamun dipaké pikeun gabung Monel K-500 boga kakuatan leuwih handap logam dasar.
Ngaran umum: Oxford Alloy® 60 FM 60 Techalloy 418
Baku: AWS 5.14 Kelas ERNiCu-7 / ASME SFA 5.14 Kelas ERNiCu-7 ASME II, SFA-5.14 UNS N04060 Werkstoff Nr. 2.4377 ISO SNi4060 Éropa NiCu30Mn3Ti
KOMPOSISI KIMIA(%)
C | Si | Mn | S | P | Ni |
≤0.15 | ≤1.25 | ≤4.0 | ≤0,015 | ≤0.02 | 62-69 |
Al | Ti | Fe | Cu | batur | |
≤1.25 | 1.5-3.0 | ≤2.5 | Istirahat | <0.5 |
PARAMETER las
Prosés | diaméterna | Voltaseu | Ampere | Gas |
TIG | .035″ (0.9mm) .045″ (1.2mm) 1/16″ (1.6mm) 3/32″ (2.4mm) 1/8″ (3.2mm) | 12-15 13-16 14-18 15-20 15-20 | 60-90 80-110 90-130 120-175 150-220 | 100% Argon 100% Argon 100% Argon 100% Argon 100% Argon |
MIG | .035″ (0.9mm) .045″ (1.2mm) 1/16″ (1.6mm) | 26-29 28-32 29-33 | 150-190 180-220 200-250 | 75% Argon + 25% Hélium 75% Argon + 25% Hélium 75% Argon + 25% Hélium |
SAW | 3/32″ (2.4mm) 1/8″ (3.2mm) 5/32″ (4.0mm) | 28-30 29-32 30-33 | 275-350 350-450 400-550 | Flux anu cocog tiasa dianggo Flux anu cocog tiasa dianggo Flux anu cocog tiasa dianggo |
Pasipatan mékanis
Kakuatan regangan | 76.5000 PSI | 530 MPA |
Kakuatan ngahasilkeun | 52.500 PSI | 360 MPA |
Elongation | 34% |
APLIKASI
ERNiCu-7 bisa dipaké pikeun aplikasi las dissimilar ngagunakeun rupa alloy nikel-tambaga nepi ka nikel 200 jeung alloy tambaga-nikel.
ERNiCu-7 dipaké pikeun gas-tungsten-arc, gas-logam-arc, sarta submerged-arc las tina alloy Monel 400 sarta K-500.
ERNiCu-7 loba dipaké dina aplikasi laut kusabab résistansi alus na kana épék corrosive of seawater jeung cai payau.
2. Kawat semprot termal séjén
Barang | Kandungan kimiawi | Zn | Cd | Pb | Fe | Cu | Balance Total |
séng murni | Nilai nominal | ≥99.995 | ≤0,002 | ≤0.003 | ≤0,002 | ≤0.001 | 0,005 |
Barang | Inconel 625 | Ni95Al5 | 45 CT | Monel 500 | HC-276 | Cr20Ni80 | |
C | ≤0.05 | ≤0.02 | 0.01-0.1 | ≤0.04 | ≤0.25 | ≤0.02 | ≤0.08 |
Mn | ≤0.4 | ≤0.2 | ≤0.2 | 2.5-3.5 | ≤1.5 | ≤1.0 | ≤0.06 |
Fe | ≤1.0 | N/A | ≤0.5 | ≤1.0 | ≤1.0 | 4.0-7.0 | N/A |
P | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.02 |
S | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.01 | ≤0.01 |
Si | ≤0.15 | ≤0.2 | ≤0.2 | ≤0.15 | ≤0.5 | ≤0.08 | 0.75-1.6 |
Cu | N/A | N/A | N/A | istirahat | 27-33 | N/A | N/A |
Ni | istirahat | istirahat | istirahat | 65-67 | istirahat | istirahat | istirahat |
Co | N/A | N/A | N/A | N/A | N/A | N/A | N/A |
Al | ≤0.4 | 4-5 | N/A | ≤0.5 | 2.3-3.15 | N/A | N/A |
Ti | ≤0.4 | 0.4-1 | 0.3-1 | 2.0-3 | 0.35-0.85 | N/A | N/A |
Cr | 21.5-23 | ≤0.2 | 42-46 | N/A | N/A | 14.5-16 | 20-23 |
Nb | 3.5-4.15 | N/A | N/A | N/A | N/A | N/A | ≤1.0 |
Mo | 8.5-10 | N/A | N/A | N/A | N/A | 15-17 | N/A |
V | N/A | N/A | N/A | N/A | N/A | ≤0.35 | N/A |
W | N/A | N/A | N/A | N/A | N/A | 3.0-4.5 | N/A |
Kotoran | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 |
3. C276kawat semprot termal
Ngaran umum: Oxford Alloy® C-276 FM C-276 Techalloy 276
Baku: AWS A5.14, ERNiCrMo-4 / ASME II, SFA-5.14, UNS N10276 Werkstoff Nr. 2.4886 ISO SNi6276 Éropa NiCrMo16Fe6W4
KOMPOSISI KIMIA(%)
C | Si | Mn | S | P | Ni | Co |
≤0.02 | ≤0.08 | ≤1.0 | ≤0.03 | ≤0.04 | Istirahat | ≤2.5 |
W | V | Fe | Cu | Cr | Mo | batur |
3.0-4.5 | ≤0.35 | 4.0-7.0 | ≤0.5 | 14.5-16.5 | 15-17 | <0.5 |
150 0000 2421